Aremco Aremco-Bond™ 807 High Performance Epoxide

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Aremco
Trade Name Aremco-Bond™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Aremco-Bond™ 807 High Performance Epoxide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
10 Minute Set, Non-Sagging, 1:1, Excellent Electrical & Mechanical Properties
Physical Properties Metric English Comments
Specific Gravity 1.39 g/cc
1.39 g/cc
Viscosity 75000 cP
75000 cP
Mixed Viscosity
Mechanical Properties Metric English Comments
Hardness, Shore D 73
73
Shear Strength 7.826 MPa
1135 psi
ASTM D1002-94
Thermal Properties Metric English Comments
CTE, linear 59.0 µm/m-°C

@Temperature 20.0 °C
32.8 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 130 °C
266 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Shrinkage 0.90 %
0.90 %
Cure Shrinkage
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+14 ohm-cm
2.00e+14 ohm-cm
Dielectric Constant 4.4

@Frequency 1000 Hz
4.4

@Frequency 1000 Hz
Dielectric Strength 15.0 kV/mm
380 kV/in
Dissipation Factor 0.030
0.030
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 23.0 °C
1.00 hour

@Temperature 73.4 °F
Pot Life 15.0 min

@Temperature 25.0 °C
15.0 min

@Temperature 77.0 °F
100 gm mass
Descriptive Properties Value Comments
Chemical Resistance Excellent
Color Gray
Mix Ratio By Weight 1:1
resin:hardener