Physical Properties Metric English Comments
Viscosity 20 - 80 cP
20 - 80 cP
Huntsman Kerimid 701-1 B US Resin
Comments/Applications: Used with Kerimid 701 A US for high Tg laminate systems. Suggested ratio 3 parts A to 1 part B.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acq..
Viscosity 70 - 80 cP

@Temperature 20.0 °C
70 - 80 cP

@Temperature 68.0 °F
4% solids aqueous solution, Hoeppler falling ball method
DuPont Elvanol® 70-75 Polyvinyl Alcohol Fully Hydrolyzed General Purpose Grade
Elvanol® polyvinyl alcohol (PVOH) is used in the manufacture of spiral wound tubes, coated paper and linerboard, and specialty water-soluble films. Its higher binding capacity versus synthetic late..
Viscosity 30 - 80 cP
30 - 80 cP
Beijing Ranger Chem 6690-3 Liquid Epoxy Resin
Information provided by Beijing Ranger Chemical Co.
Viscosity 40 - 80 cP
40 - 80 cP
Aremco Glass-Coat™ SGC4000 High Temperature Specialty Coatings Silicone-Glass
Silicone-glass-ceramic, gray, low viscosity, scratch resistant coating for stainless steel to 900°F (482°C)
Viscosity 40 - 80 cP
40 - 80 cP
3M Scotch-Weld™ 2290 Epoxy Adhesive/Coating
3M™ Scotch-Weld™ Epoxy Adhesive/Coating 2290 is an amber tinted thermo-setting adhesive/coating for metal to metal bonding and coating. It can be used to assemble laminated steel cores for electri..