Gwent Electronic Materials C2080815P1 Silver Flexographic Ink

Category Fluid , Metal , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Gwent Electronic Materials Ltd.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gwent Electronic Materials C2080815P1 Silver Flexographic Ink.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Silver conductor ink specifically designed for printing on to polymeric or paper substrates using flexographic printing. Ink can be printed at speeds up to 20m/min, with good line definition and good conductivity.Testing was carried out on a Timsons T-Flex 508 and Nilpeter FB-3300.Substrate: Polyester, PVC, BOPP, Cellophane, Paper or Cellulosic BoardInformation provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Solids Content 66 - 68 %

@Temperature 700 °C
66 - 68 %

@Temperature 1290 °F
Viscosity 800 - 1000 cP

@Shear Rate 50.0 1/s,
Temperature 25.0 °C
800 - 1000 cP

@Shear Rate 50.0 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Storage Temperature 20.0 °C
68.0 °F
sealed container
Electrical Properties Metric English Comments
Volume Resistivity 0.000065 ohm-cm
0.000065 ohm-cm
printed onto 125µm PET film using 18cm<sup>3</sup>m<sup>-2</sup> anilox
Surface Resistivity per Square 0.025 - 0.030 ohm

@Thickness 0.0250 mm
0.025 - 0.030 ohm

@Thickness 0.000984 in
printed onto 125µm PET film using 18cm<sup>3</sup>m<sup>-2</sup> anilox
0.15 - 0.165 ohm

@Thickness 0.00400 mm
0.15 - 0.165 ohm

@Thickness 0.000157 in
Printed onto 125µm PET film using 18cm<sup>3</sup>m<sup>-2</sup> anilox
Processing Properties Metric English Comments
Shelf Life 6.00 Month
6.00 Month