Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.0240 g/cc | 0.000867 lb/in³ | On a continuous pre-expander after one expansion |
Polimeri Europa Extir® E 2000 AE Expandable Polystyrene
(discontinued **) Extir E 2000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of fine particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. Thi.. |
|||
Apparent Bulk Density | 0.0240 g/cc | 0.000867 lb/in³ | On a continuous pre-expander after one expansion |
Polimeri Europa Extir® F 1111 Expandable Polystyrene
(discontinued **) Extir F 1111 is an expandable polystyrene in the form of spherical beads of very fine particle size and a narrow particle size distribution, containing pentane as blowing agent. Extir does not cont.. |