Physical Properties Metric English Comments
Apparent Bulk Density 0.0240 g/cc
0.000867 lb/in³
On a continuous pre-expander after one expansion
Polimeri Europa Extir® E 2000 AE Expandable Polystyrene  (discontinued **)
Extir E 2000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of fine particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. Thi..
Apparent Bulk Density 0.0240 g/cc
0.000867 lb/in³
On a continuous pre-expander after one expansion
Polimeri Europa Extir® F 1111 Expandable Polystyrene  (discontinued **)
Extir F 1111 is an expandable polystyrene in the form of spherical beads of very fine particle size and a narrow particle size distribution, containing pentane as blowing agent. Extir does not cont..