Physical Properties | Metric | English | Comments |
---|---|---|---|
Pore Size | 12.7 - 15.2 microns | 0.500 - 0.600 mil | Average value: 13.5 microns Grade Count:3 |
Overview of materials for Epoxy, Cast, Metal Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a.. |