Physical Properties Metric English Comments
Pore Size 12.7 microns
0.500 mil
Mean pore diameter
CMT Materials METAPOR® HD 100 AL Air Permeable Material
METAPOR® is a composite material made of aluminum granules and epoxy resin. The material is air-permeable over the entire surface due to its micro-porous structure allowing for unique design consi..
Pore Size 12.7 microns
0.500 mil
Mean pore diameter
CMT Materials METAPOR® HD 210 AL Air Permeable Material
METAPOR® is a composite material made of aluminum granules and epoxy resin. The material is air-permeable over the entire surface due to its micro-porous structure allowing for unique design consi..
Pore Size 12.7 - 15.2 microns
0.500 - 0.600 mil
Average value: 13.5 microns Grade Count:3
Overview of materials for Epoxy, Cast, Metal Filled
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a..