Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.40 - 0.75 g/10 min | 0.40 - 0.75 g/10 min | ±18% |
Kazanorgsintez 297-285 High Density Polyethylene Composite Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions 296-.. |
|||
Melt Flow | 0.40 - 0.75 g/10 min | 0.40 - 0.75 g/10 min | ±18% |
Kazanorgsintez 297-285D High Density Polyethylene Composite Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions 296-.. |