ExxonMobil LDPE LD 159AC Low Density Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Exxon Chemical
Trade Name LDPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LDPE LD 159AC Low Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: LD 159AC is an LDPE grade, which offers good draw down combined with good mechanical strength. Availability: Africa & Middle East and Europe Additive: Antiblock: 450 ppmSlip: 500 ppmThermal Stabilizer: YesApplications: Blend PartnerCo-extrusion FilmsCollation ShrinkFood packagingForm Fill and Seal PackagingFreezer FilmLamination FilmMedium Duty Shrink FilmProduce BagsShoppersInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.924 g/cc
0.0334 lb/in³
ExxonMobil method
Melt Flow 1.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 450 ppm
450 ppm
Slip Level 500 ppm
500 ppm
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 340 %
340 %
ASTM D882
Film Elongation at Break, TD 550 %
550 %
ASTM D882
Elmendorf Tear Strength MD 290 g
290 g
ASTM D1922
Elmendorf Tear Strength TD 220 g
220 g
ASTM D1922
Dart Drop Test 140 g
0.309 lb
ASTM D1709A
Film Tensile Strength at Break, MD 20.7 MPa
3000 psi
ASTM D882
Film Tensile Strength at Break, TD 20.7 MPa
3000 psi
ASTM D882
1% Secant Modulus, MD 221 MPa
32000 psi
ASTM D882
1% Secant Modulus, TD 248 MPa
36000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point <= 228 °C
<= 442 °F
Peak Melting Point; ExxonMobil method
Optical Properties Metric English Comments
Haze 6.0 %
6.0 %
ASTM D1003
Gloss 73 %
73 %
45°; ASTM D2457