Material Notes:
WESTLAKE low-density polyethylene EC850 is a resin designed for applications where high coating speeds and good drawdown are required. The combination of high melt index and low density provides good heat seals at high packing or sealing rates. It also demonstrates good adhesion to paper, provides a good moisture barrier, and is heat-sealable at low temperatures.Application/UsesCoatings for paper/paperboardFood contact applicationsFDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.915 g/cc
0.0331 lb/in³
ASTM D1505
Melt Flow 12.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
12.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 9.70 MPa
1410 psi
500mm/min; ASTM D638 Type IV Specimen
Elongation at Break 400 %
400 %
500mm/min; ASTM D638 Type IV Specimen
2% Secant Modulus 0.172 GPa
24.9 ksi
12.7mm/min; ASTM D790
Processing Properties Metric English Comments
Melt Temperature 149 - 166 °C
300 - 330 °F
Descriptive Properties Value Comments
Process Coating
Region US & Canada
Bamberger Polymers Distribution