Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.8 - 2.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.8 - 2.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Kazanorgsintez PE2NT75-15 High Density Polyethylene for Blow Molding Production Method: Gaseous-phase method. Application: Compositions are intended for goods produced by injection molding method.Information Provided by Kazanorgsintez |
|||
Melt Flow | 2.2 - 2.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 - 2.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical SEETEC ST408 Linear Low Density Polyethylene, Blown Film Grade Features: Characteristics- Excellent puncture resistance, tear strength. Excellent sealing and optical properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplica.. |