Physical Properties Metric English Comments
Melt Flow 29 g/10 min
29 g/10 min
I<sub>21</sub>; ASTM D238
Petromont 1000 High Density Polyethylene Resin
Petromont HDPE 1000 is a high density polyethylene copolymer resin produced using the Unipol® Process. This multi-purpose resin can be used on intermittent and continuous blow moulding machines to ..
Melt Flow 29 g/10 min
29 g/10 min
I<sub>21</sub>; ASTM D238
Petromont 1002 High Density Polyethylene Resin
Petromont HDPE 1002 is a blow moulding high-density polyethylene copolymer resin produced using the UNIPOL® Process. This multi-purpose resin can be used on intermittent and continuous extrusion bl..
Melt Flow 29 g/10 min
29 g/10 min
ISO 1133
Solvay Engineered Polymers SEQUEL® 1402 TPO  (discontinued **)
Description: SEQUEL® 1402 engineered polyolefin material is designed for large automotive exterior applications that require high melt flow, excellent paintability, and processability. Applications..
Melt Flow 29 g/10 min

@Load 2.16 kg,
Temperature 260 °C
29 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D1238
SABIC Innovative Plastics GELOY XTPMFR10 ASA+PC (Asia Pacific)
Improved ASA/PC blend for high flow, 1.0mm V0 applications. Improved UV performance aesthetically and physically compared to alternatives.
Melt Flow 29 g/10 min

@Load 5.00 kg,
Temperature 190 °C
29 g/10 min

@Load 11.0 lb,
Temperature 374 °F
Total Finaprene® 411x Styrene-Butadiene TPE Copolymer Compounded to 58 Shore A  (discontinued **)
Styrene-Butadiene CopolymerDescription: Finaprene® 411x is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its high molecular weight, Finaprene® 411x provides e..
Melt Flow 29 g/10 min

@Load 1.20 kg,
Temperature 300 °C
29 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® BFL2000B PC (Asia Pacific)
Lexan BFL2000B resin is a Br- & Cl-free FR polycarbonate resin featuring high flow with balanced impact. It is available only in dark colors.
Melt Flow 29 g/10 min

@Load 1.20 kg,
Temperature 224 °C
29 g/10 min

@Load 2.65 lb,
Temperature 435 °F
Dow Pellethane® 2102-90AE Polyurethane Elastomer, Polyester Polycaprolactone Based  (discontinued **)
PELLETHANE® 2102-90AE elastomer is a polyester polycaprolactone based polyurethane elastomer which combines excellent resistance to fuels and oils with good damping capacity and good hydrolytic sta..
Melt Flow 29 g/10 min

@Load 2.16 kg,
Temperature 330 °C
29 g/10 min

@Load 4.76 lb,
Temperature 626 °F
cm³/10 min.
Covestro Apec® 1605 Polycarbonate  (discontinued **)
Key Features:Release agentUnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingCalanderingTransfer moldingThermoformingInformation pr..
Melt Flow 29 g/10 min
29 g/10 min
ISO 1133
LyondellBasell SEQUEL® 1480 Engineered Polyolefin
Description: SEQUEL® 1480 engineered polyolefin material is designed for large automotive exterior applications that require ductile impact properties at low temperatures, excellent paintability,..
Melt Flow 29 g/10 min

@Load 2.16 kg,
Temperature 230 °C
29 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
LyondellBasell Integrateâ„¢ NP507030 Functionalized Polyolefin
INTEGRATE products are chemically modified polyolefins used to combine dissimilar materials for a variety of applications including molding articles, flexible materials and fiber technology or to pr..
Melt Flow 29 g/10 min

@Load 5.00 kg,
Temperature 200 °C
29 g/10 min

@Load 10.8 lb,
Temperature 392 °F
Kraton® D1117 P (SIS) Linear Block Copolymer
Description:Kraton D1117 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 17%. It is supplied from North America in the physical form identified: K..
Melt Flow 29 g/10 min

@Load 5.00 kg,
Temperature 200 °C
29 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Kraton® D1117 P (SIS) Linear Triblock Copolymer
Description: Kraton D1117 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 17%. It is supplied from North America in the physical form identified: ..
Melt Flow 29 g/10 min

@Load 2.16 kg,
Temperature 230 °C
29 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Kuraray SEPTON® PM1 Polypropylene Modified Plastic
Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are a series of hydrogenated styrenic blo..
Melt Flow 29 g/10 min

@Load 2.16 kg,
Temperature 260 °C
29 g/10 min

@Load 4.76 lb,
Temperature 500 °F
Calculated from MVR using melt density; ISO 1133
Lanxess Pocan® KL 1-7265 000000 PBT, 15% Glass Fiber
PBT, 15% glass fibers, injection molding
Melt Flow 29 g/10 min

@Load 5.00 kg,
Temperature 260 °C
29 g/10 min

@Load 11.0 lb,
Temperature 500 °F
Calculated from MVR using melt density; ISO 1133
Lanxess Durethan® BKV 115 000000 Copolyamide, 15% Glass Fiber
CoPA, injection molding grade, 15% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 15, even in..
Melt Flow 29 g/10 min

@Load 10.0 kg,
Temperature 220 °C
29 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Samsung Cheil Industries Starex® LX-0951 ABS, Unreinforced Metallic-Look
Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries.
Melt Flow 29 g/10 min

@Load 10.0 kg,
Temperature 220 °C
29 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Samsung Cheil Industries Starex® LX-0951 ABS, Unreinforced Metallic-Look
Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries.
Melt Flow 29 g/10 min

@Load 2.16 kg,
Temperature 230 °C
29 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
A. Schulman POLYFORT™ PP 3726
Information provided by A. Schulman.
Melt Flow 29 g/10 min

@Load 2.16 kg,
Temperature 230 °C
29 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
A. Schulman POLYFORT™ PP 3726
Information provided by A. Schulman.
Melt Flow 29 g/10 min

@Load 2.16 kg,
Temperature 230 °C
29 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
A. Schulman POLYFORT™ PP 3726
Information provided by A. Schulman.
Melt Flow 29 g/10 min

@Load 2.16 kg,
Temperature 230 °C
29 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
A. Schulman POLYFORT™ PP 3726
Information provided by A. Schulman.
Melt Flow 29 g/10 min

@Load 2.16 kg,
Temperature 230 °C
29 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
A. Schulman POLYFORT™ PP 3726
Information provided by A. Schulman.
Melt Flow 29 g/10 min

@Load 5.00 kg,
Temperature 260 °C
29 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ISO 1133
Covestro Makroblend® DP UT5005 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendimpact modifiedeasy releaseinjection molding gradeMakroblend DP UT5005* provides an outstanding balance of low-temperature impact strength and flowability beside e..
Melt Flow 29 g/10 min

@Load 5.00 kg,
Temperature 260 °C
29 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ISO 1133
Covestro Makroblend® DP UT5007 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendimpact modifiedeasy releaseUV-stabilizedinjection molding grade Makroblend DP UT5007* provides an outstanding balance of low-temperature impact strength and flow..
Melt Flow 29 g/10 min

@Load 5.00 kg,
Temperature 265 °C
29 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
Diamond Polymers ABSPC 7801 ABS/PC Injection Molding Grade, High Impact, High Heat
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Melt Flow 29 g/10 min

@Load 2.16 kg,
Temperature 190 °C
29 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Braskem IC32 LLDPE Injection Molding Polyethylene Copolymer
IC32 is a linear low-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding. It offers good fluidity, excellent flexibility and tenac..
Melt Flow 29 g/10 min

@Load 10.0 kg,
Temperature 360 °C
29 g/10 min

@Load 22.0 lb,
Temperature 680 °F
ISO 1133
BASF Ultrason E 2010 G4 20% Glass Filled PES
Ultrason E 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength.
Melt Flow 29 g/10 min

@Load 2.16 kg,
Temperature 230 °C
29 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
A. Schulman POLYFORT™ PP 3726
Information provided by A. Schulman.
Copyright © lookpolymers.com All Rights Reserved