Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 23 - 29 g/10 min @Load 2.16 kg, Temperature 190 °C |
23 - 29 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem PH 2610 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Melt Flow | 23 - 29 g/10 min @Load 2.16 kg, Temperature 235 °C |
23 - 29 g/10 min @Load 4.76 lb, Temperature 455 °F |
ASTM D1238 |
Gromax PBT 1100-211L Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Melt Flow | 21 - 29 g/10 min @Load 2.16 kg, Temperature 280 °C |
21 - 29 g/10 min @Load 4.76 lb, Temperature 536 °F |
Z-011A |
Zeon Chemicals Zeonex® E48R Cyclo-Olefin Polymer |
|||
Melt Flow | 5.0 - 29 g/10 min @Load 3.80 kg, Temperature 232 °C |
5.0 - 29 g/10 min @Load 8.38 lb, Temperature 450 °F |
ASTM D1238 |
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Melt Flow | 5.0 - 29 g/10 min @Load 3.80 kg, Temperature 232 °C |
5.0 - 29 g/10 min @Load 8.38 lb, Temperature 450 °F |
ASTM D1238 |
Arkema Group KYNAR® 721 Polyvinylidene Fluoride Powder Characteristics: White, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistan.. |