Physical Properties Metric English Comments
Melt Flow 29.4 g/10 min

@Load 2.16 kg,
Temperature 260 °C
29.4 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ISO 1133
Topas Advanced Polymers TOPAS® 8007D-61 Cyclic Olefin Copolymer (COC)
TOPAS® 8007D-61 is an externally lubricated version of our 8007 series of injection molding resins, targeting injection blow molding (IBM) and injection stretch blow molding (ISBM) applications. Li..
Melt Flow 29.4 g/10 min

@Load 2.16 kg,
Temperature 260 °C
29.4 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ISO 1133
Topas Advanced Polymers TOPAS® 8007S-04 Cyclic Olefin Copolymer (COC)
TOPAS® 8007S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma..
Melt Flow 29.4 g/10 min

@Load 2.16 kg,
Temperature 260 °C
29.4 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ISO 1133
Topas Advanced Polymers TOPAS® 8007X10 Cyclic Olefin Copolymer (COC)
TOPAS® 8007X10 is a highly UV-transparent version of our 8007 series of injection molding resins. Like the rest of the 8007 grades, 8007X10 is a glass-clear amorphous polymer with outstanding moist..
Melt Flow 29.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
29.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
BASF Ultraform W 2320 003 UNC Q600 POM
Ultraform W2320 003 UNC Q600 is a very easy flowing and rapidly solidifying injection molding POM grade for use where processing is extremely difficult but mechanical properties are lower. Contains ..
Melt Flow 29.4 g/10 min

@Load 2.16 kg,
Temperature 275 °C
29.4 g/10 min

@Load 4.76 lb,
Temperature 527 °F
ISO 1133
BASF Ultradur® S 4090 G6X 30% Glass Filled PBT
Description: Is a PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 30% of glass fibers for industrial parts with high dimensional stab..