Physical Properties Metric English Comments
Melt Flow 49 g/10 min

@Load 5.00 kg,
Temperature 230 °C
49 g/10 min

@Load 11.0 lb,
Temperature 446 °F
Advanced Elastomer Systems VistaFlex® 715-N Thermoplastic Rubber  (discontinued **)
Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f..
Melt Flow 49 g/10 min

@Load 5.00 kg,
Temperature 300 °C
49 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics NORYL V03505 PPE+HIPS
Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Melt Flow 49 g/10 min

@Load 5.00 kg,
Temperature 300 °C
49 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Asia Pacific)
Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Melt Flow 49 g/10 min

@Load 5.00 kg,
Temperature 300 °C
49 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Europe-Africa-Middle East)
Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Melt Flow 49 g/10 min

@Load 10.0 kg,
Temperature 250 °C
49 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Samsung Cheil Industries Infino® HA-1011 PC/ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Melt Flow 49 g/10 min

@Load 10.0 kg,
Temperature 250 °C
49 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Samsung Cheil Industries Infino® HA-1011 PC/ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Melt Flow 49 g/10 min

@Load 1.20 kg,
Temperature 224 °C
49 g/10 min

@Load 2.65 lb,
Temperature 435 °F
ASTM D1238
Lubrizol Estane® 2102-65D Thermoplastic Polyurethane Elastomer
Formerly PellethaneAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
Melt Flow 49 g/10 min

@Load 10.0 kg,
Temperature 190 °C
49 g/10 min

@Load 22.0 lb,
Temperature 374 °F
ISO 1133
BASF Ultraform® FK 66003 20% Silicone Filled POM
Description: Polyoxymethylene based batch with approx. 20% silicone (polysiloxane) for modifying tribological properties of thermoplastic polyoxymethylenes. Recommended concentrations of batch FK660..
Melt Flow 49 g/10 min

@Load 5.00 kg,
Temperature 270 °C
49 g/10 min

@Load 11.0 lb,
Temperature 518 °F
Calculated from MVR using melt density; ISO 1133
Lanxess Pocan® S 7020 000000 PBT
PBT, non-reinforced, injection molding, extrusion, flame retardant, impact modified