Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 55.0 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 0.0100 - 55.0 g/10 min
0.0100 - 55.0 g/10 min
Average value: 5.89 g/10 min Grade Count:267
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum..
Melt Flow 0.0270 - 55.0 g/10 min
0.0270 - 55.0 g/10 min
Average value: 4.97 g/10 min Grade Count:158
Overview of materials for High Density Polyethylene (HDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max..
Melt Flow 1.00 - 55.0 g/10 min
1.00 - 55.0 g/10 min
Average value: 13.1 g/10 min Grade Count:32
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max..
Melt Flow 0.500 - 55.0 g/10 min
0.500 - 55.0 g/10 min
Average value: 3.58 g/10 min Grade Count:32
Overview of materials for Linear Low Density Polyethylene (LLDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Blow Molding Grade". Each property range of values reported is ..
Melt Flow 4.50 - 55.0 g/10 min
4.50 - 55.0 g/10 min
Average value: 17.8 g/10 min Grade Count:22
Overview of materials for Polycarbonate, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app..