Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.0100 - 55.0 g/10 min | 0.0100 - 55.0 g/10 min | Average value: 5.89 g/10 min Grade Count:267 |
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum.. |
|||
Melt Flow | 0.0270 - 55.0 g/10 min | 0.0270 - 55.0 g/10 min | Average value: 4.97 g/10 min Grade Count:158 |
Overview of materials for High Density Polyethylene (HDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max.. |
|||
Melt Flow | 1.00 - 55.0 g/10 min | 1.00 - 55.0 g/10 min | Average value: 13.1 g/10 min Grade Count:32 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Melt Flow | 0.500 - 55.0 g/10 min | 0.500 - 55.0 g/10 min | Average value: 3.58 g/10 min Grade Count:32 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Blow Molding Grade". Each property range of values reported is .. |
|||
Melt Flow | 4.50 - 55.0 g/10 min | 4.50 - 55.0 g/10 min | Average value: 17.8 g/10 min Grade Count:22 |
Overview of materials for Polycarbonate, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app.. |