Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.300 - 58.0 g/10 min | 0.300 - 58.0 g/10 min | Average value: 13.3 g/10 min Grade Count:92 |
Overview of materials for Polyether Ester Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr.. |
|||
Melt Flow | 9.59 - 58.0 g/10 min | 9.59 - 58.0 g/10 min | Average value: 25.7 g/10 min Grade Count:18 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |