Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.10 - 6.00 g/10 min | 2.10 - 6.00 g/10 min | Average value: 3.78 g/10 min Grade Count:5 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Wire/Cable Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Wire/Cable Grade". Each property range of values reported is min.. |
|||
Melt Flow | 1.00 - 6.00 g/10 min | 1.00 - 6.00 g/10 min | Average value: 2.90 g/10 min Grade Count:5 |
Overview of materials for Low Density Polyethylene (LDPE), Sheet/Profile extrusions This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Sheet/Profile extrusions". Each property range of values reported is mi.. |
|||
Melt Flow | 1.70 - 6.00 g/10 min | 1.70 - 6.00 g/10 min | Average value: 3.52 g/10 min Grade Count:26 |
Overview of materials for High Density Polyethylene (HDPE), Rotational Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Rotational Molding Grade". Each property range of values reported is m.. |