Physical Properties Metric English Comments
Melt Flow 2.10 - 6.00 g/10 min
2.10 - 6.00 g/10 min
Average value: 3.78 g/10 min Grade Count:5
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Wire/Cable Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Wire/Cable Grade". Each property range of values reported is min..
Melt Flow 1.00 - 6.00 g/10 min
1.00 - 6.00 g/10 min
Average value: 2.90 g/10 min Grade Count:5
Overview of materials for Low Density Polyethylene (LDPE), Sheet/Profile extrusions
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Sheet/Profile extrusions". Each property range of values reported is mi..
Melt Flow 1.70 - 6.00 g/10 min
1.70 - 6.00 g/10 min
Average value: 3.52 g/10 min Grade Count:26
Overview of materials for High Density Polyethylene (HDPE), Rotational Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Rotational Molding Grade". Each property range of values reported is m..