Physical Properties Metric English Comments
Cell Length 0.700 - 1.60 mm
0.0276 - 0.0630 in
Zotefoams Plastazote® HD110 High Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Cell Length 0.900 - 1.60 mm
0.0354 - 0.0630 in
Zotefoams Plastazote® LD24LC Low Density Polyethylene Foam, Large Cell
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Cell Length 0.700 - 1.60 mm
0.0276 - 0.0630 in
Zotefoams Plastazote® HD115 High Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Cell Length 0.900 - 1.60 mm
0.0354 - 0.0630 in
Zotefoams Plastazote® LD33LC Low Density Polyethylene Foam, Large Cell
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..