Physical Properties | Metric | English | Comments |
---|---|---|---|
Cell Length | 0.900 - 1.60 mm | 0.0354 - 0.0630 in | |
Zotefoams Plastazote® LD24LC Low Density Polyethylene Foam, Large Cell Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Cell Length | 0.900 - 1.60 mm | 0.0354 - 0.0630 in | |
Zotefoams Plastazote® LD33LC Low Density Polyethylene Foam, Large Cell Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Cell Length | 0.900 mm | 0.0354 in | Typical Diameter |
Zotefoams Plastazote® MP15FR Metallocene Polyethylene Foam, Flame Retardant Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |