Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 254 - 305 microns
10.0 - 12.0 mil
Overall
Arlon R31901R011 0.011" (0.279 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place..
Thickness 254 - 305 microns
10.0 - 12.0 mil
Overall
Arlon R34931R010 0.011" (0.279 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place ..
Thickness 254 - 305 microns
10.0 - 12.0 mil
Overall
Arlon 44571B010 0.011" (0.279 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data represents typical values for the production material. The data should not be used to write, or in place..
Thickness 254 - 305 microns
10.0 - 12.0 mil
Overall
Arlon 44571R010 0.011" (0.279 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. T..
Thickness 229 - 305 microns
9.00 - 12.0 mil
Overall; Arlon SQA-TMS-003
Arlon 49091R010 0.0105" (0.267 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data Represents typical values for the production material. The data s..
Thickness 229 - 305 microns
9.00 - 12.0 mil
Overall
Arlon 912-10RXX-P0 0.012" (0.305 mm) Self-Fusing Silicone Tape
Design/Construction:Cross Section Type: RectangularArlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape is not required.P..