Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 229 microns | 9.00 mil | cured laminate, per ply |
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, 7781 E-Glass Reinforced Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock.. |
|||
Thickness | 229 microns | 9.00 mil | |
Hexcel® HexForce™ 7581 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 229 - 279 microns | 9.00 - 11.0 mil | Overall |
Arlon 10502R010 0.010" (.254 mm) Cured/Post-Cured Unsupported Silicone Rubber Design/Construction:Side 1: Cured/Post-Cured Unsupported Silicone RubberAppearance: Red silicone rubberThis data represents typical values for the production material. The data should not be used to.. |
|||
Thickness | 229 microns | 9.00 mil | side 2 silicone; Arlon SQA-TMS-003 |
Arlon 51106RB015D Silicone Rubber/Fiberglass Laminate Interleave 2: 3 mil PE; Side 2: cured silicone rubber; Substrate: 7628 fiberglass; Side 1: uncured silicone rubber, Interleave 1: 3 mil PE |
|||
Thickness | 229 microns | 9.00 mil | Layer 2; Arlon SQA-TMS-003 |
Arlon 51629R020 0.020" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil polyLayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production mat.. |
|||
Thickness | 229 microns | 9.00 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 55586R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: PolyethyleneAppearance: Red silicone gum and rubber on fiberglass clothTh.. |
|||
Thickness | 229 microns | 9.00 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 56810R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone Rubber Substrate: 1564 Style Fiberglass This data represents typical values for the production material. The data should not be.. |
|||
Thickness | 229 microns | 9.00 mil | Tape |
3M XR4123 Double Coated Film Tape 3M™ X-Series Industrial Attachment Tapes offer a variety of performance characteristics and product constructions to support demanding application requirements. This product line provides a range o.. |
|||
Thickness | 229 microns | 9.00 mil | |
Aremco Pyro-Tape™ 682-AR High Temperature Tape Single-layer ultra-high molecular weight polyethylene with a rubber adhesive Applications Abrasion Resistance Features Low coefficient of friction to reduce wear, scratching and noise. Liners for chutes, rails and slides. |
|||
Thickness | 229 - 279 microns | 9.00 - 11.0 mil | Overall |
Arlon 30580R010 0.010" (0.254 mm) Uncured/Unsupported Silicone Rubber on a Release Carrier Design/Construction:Side 1: Uncured/Unsupported Silicone Rubber on a Release Carrier Appearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The.. |
|||
Thickness | 229 - 305 microns | 9.00 - 12.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 49091R010 0.0105" (0.267 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data Represents typical values for the production material. The data s.. |
|||
Thickness | 229 microns | 9.00 mil | side 2 silicone; Arlon SQA-TMS-003 |
Arlon 51106R020 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Thickness | 229 microns | 9.00 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 51271R037 0.037" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 2.5 mil PolyethyleneThis data represents typical values for the produ.. |
|||
Thickness | 229 microns | 9.00 mil | side 2; Arlon SQA-TMS-003 |
Arlon 51276R020 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Thickness | 229 microns | 9.00 mil | Layer 2; Arlon SQA-TMS-003 |
Arlon 51279R020 0.020" (0.508 mm) Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass This data represents typical values for the production ma.. |
|||
Thickness | 229 microns | 9.00 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 51986RA020 0.020" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PolyethyleneThis data represents typical values for the producti.. |
|||
Thickness | 229 microns | 9.00 mil | side 1; Arlon SQA-TMS-003 |
Arlon 53423R032 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 1: cured silicone rubber; Substrate: 2523 fiberglass; Side 2: cured silicone rubber |
|||
Thickness | 229 microns | 9.00 mil | side 2; Arlon SQA-TMS-003 |
Arlon 53423R032 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 1: cured silicone rubber; Substrate: 2523 fiberglass; Side 2: cured silicone rubber |
|||
Thickness | 229 - 381 microns | 9.00 - 15.0 mil | Overall |
Arlon 912-10C16.4FR-P0 0.012" (0.305 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularRoll Length: 16.4 Yards Width, inches: 1Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smoo.. |
|||
Thickness | 229 microns | 9.00 mil | Tape Caliper |
3M 9579 Double Coated Tape with Adhesive 760 3M™ Double Coated Tape 9579 with 3M™ Adhesive 760 is a high-tack, hand-tearable, double coated film tape with a pressure sensitive adhesive on each side of the carrier. The medium firm adhesive fe.. |
|||
Thickness | >= 229 microns | >= 9.00 mil | Side 2 |
Arlon R33826R017 0.017" (0.432mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Thickness | 229 microns | 9.00 mil | Tape Caliper |
3M 9589 Double Coated Tapes with Adhesive 700 Series 3M™ Double Coated Tapes with 3M™ Adhesive 700 Series feature a high tack synthetic rubber adhesive which provides excellent quick stick or initial adhesion and bonds together a wide variety of mat.. |
|||
Thickness | 229 - 279 microns | 9.00 - 11.0 mil | Overall |
Arlon 44250R011 0.011" (0.279 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. The data should not be used to wri.. |
|||
Thickness | 229 - 279 microns | 9.00 - 11.0 mil | Overall |
Arlon 44560R009W 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Appearance Red silicone gum on glass fabricThis data represents typical values for the production material. The data should not be used to write, .. |
|||
Thickness | 229 - 279 microns | 9.00 - 11.0 mil | Overall |
Arlon 44570B010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Layers Silicone Rubber This data represents typical values for the production material. The data should not be used to write, or in place of, material specificati.. |
|||
Thickness | 229 - 1140 microns | 9.00 - 45.0 mil | |
Alcoa KAMA SealPET™ 4205 RF Sealable RPET
(discontinued **) CapabilitiesGauge: .009” to .045” (229 to 1143 µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Silicone coating a.. |
|||
Thickness | 229 - 279 microns | 9.00 - 11.0 mil | Overall |
Arlon 30600R010 0.010" (0.254 mm) Uncured/Unsupported Silicone Rubber on a Release Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on a Release Carrier Product Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThis.. |
|||
Thickness | 229 - 279 microns | 9.00 - 11.0 mil | Side 1 |
Arlon 30600R010 0.010" (0.254 mm) Uncured/Unsupported Silicone Rubber on a Release Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on a Release Carrier Product Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThis.. |
|||
Thickness | 229 microns | 9.00 mil | side 2; Arlon SQA-TMS-003 |
Arlon R37806X030 Silicone Rubber/Fiberglass Interleave: 3 mil PE; Side 2: uncured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber |