Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 3180 - 12700 microns | 125 - 500 mil | Range of Thicknesses Available |
Rogers Corporation Poron® 4790-92-15 Urethane Foam, Extra Soft, Slow Rebound Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
Thickness | 3180 - 12700 microns | 125 - 500 mil | Range of Thicknesses Available |
Rogers Corporation Poron® Shock Seal™ 4790-79-15 Urethane Foam, Industrial Grade Thickness: 0.125"- 0.500"Color: BlackInformation provided by Rogers Corporation. |
|||
Thickness | 3180 microns | 125 mil | Gauge, nominal |
Mid-Mountain Materials ARMATEX® SF90 Silicone Rubber Coated Glass Fabric Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based... |
|||
Thickness | 3180 - 25400 microns | 125 - 1000 mil | nom |
Mid-Mountain Materials PADMAT® MT1000 Needled Fiberglass Mat Description: PADMAT® MT1000 fiberglass mat is comprised of high purity, high strength E-Glass fibers. These long fibers are mechanically needled into high strength, binderless insulation material.. |
|||
Thickness | 3180 microns | 125 mil | injection molded |
Dow AFFINITY™ SM 1300G Polyolefin Plastomer (POP) AFFINITY™ SM 1300G is an ethylene alpha-olefin resin for Injection Molding is produced via INSITE™ Technology from Dow Plastics. The resin offers excellent performance in durable injection molded.. |
|||
Thickness | 3180 microns | 125 mil | Total |
3M 4318 Single-Coated Foam Tape 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast.. |
|||
Thickness | 3180 microns | 125 mil | |
3M 4508 Foam Tape Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio.. |
|||
Thickness | 3180 microns | 125 mil | Overall |
Arlon 10842N125 Cured/Post-cured, Unsupported Silicone Rubber Low ModulusProduct Color: Natural (Transparent)Interleave: 0.003" PolyethyleneThis data represents typical values for the production material and should not be used as material specifications.Inform.. |
|||
Thickness | 3180 microns | 125 mil | Overall |
Arlon 10842R125 Cured/Post-cured, Unsupported Silicone Rubber Low ModulusProduct Color: RedInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should not be used as material specifications.Information provided by .. |
|||
Thickness | 3180 microns | 125 mil | Overall |
Arlon 10842S125 Cured/Post-cured, Unsupported Silicone Rubber Low ModulusProduct Color: Saddle BrownInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should not be used as material specifications.Information pro.. |
|||
Thickness | 3180 microns | 125 mil | Overall Thickness |
Arlon 27122T125 Cured Silicone Rubber/Skive Tape Laminate Design/Construction:Side 1: Cured Silicone RubberSubstrate: 5.0 mil Etched Skive Tape bonded to one sideThis data represents typical values for the production material and should not be used as ma.. |
|||
Thickness | 3180 microns | 125 mil | |
3M Bumpon™ SJ5208 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Thickness | 3180 microns | 125 mil | |
3M Bumpon™ SJ5908 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Thickness | 3180 microns | 125 mil | |
3M Bumpon™ SJ6008 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Thickness | 3180 microns | 125 mil | Overall; Arlon SQA-TMS-003 |
Arlon Ultrapad™ 55072R125D 0.125" (3.17 mm) Cured Silicone Rubber with Fiberglass Substrate Description: Ultrapad™ Silicone-based press pad. Arlon UltraPad press pad is a high performance, fiberglass reinforced, silicone sheet designed for flex and rigid-flex circuitry lamination. UltraPa.. |
|||
Thickness | 3180 microns | 125 mil | Dry |
3M Scotchkote™ GP 120 Epoxy Primer Scotchkote Epoxy Primer GP 120 has been specifically developed as an anti corrosive coating for steel structures that cannot be abrasive blast cleaned.Product Features:Suitable for use on mechanical.. |
|||
Thickness | 3180 microns | 125 mil | ASTM D1000 |
3M Scotch-Seal™ 2229 Mastic Tape and Pads 3M™ Scotch-Seal™ Mastic Tape and Pads 2229 are conformable, durable, tacky mastic coated on an easy release liner. The product is designed for quick and easy insulating, padding and sealing of obj.. |
|||
Thickness | 3180 microns | 125 mil | Composite-Pad; ASTM D1000 |
3M Scotch™ 2200 Vinyl Mastic Pads and Rolls 3M™ Scotch™ Brand 2200 Pads and 2210 Rolls are self fusing, rubber based insulating compounds laminated to a flexible, all weather grade vinyl (PVC) backing. These tape rolls and precut pads are d.. |
|||
Thickness | 3180 microns | 125 mil | Rubber |
Arlon 30850S125 0.125" Uncured, Unsupported Silicone Rubber on a Kodacel Carrier Design/Construction:Side 1: Uncured, Unsupported Silicone RubberSubstrate: Kodacel CarrierInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should.. |
|||
Thickness | 3180 microns | 125 mil | |
3M 4008 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |
|||
Thickness | 3180 microns | 125 mil | Total |
3M 4108 Single-Coated Foam Tape 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast.. |
|||
Thickness | 3180 microns | 125 mil | ASTM D1000 |
3M Scotchfil™ Electrical Insulation Putty 3M™ Scotchfil™ Electrical Insulation Putty is used as a build-up compound on highly irregular surfaces such as fittings and valves, providing a smooth, waterproof taping surface. The putty is soft.. |
|||
Thickness | 3180 microns | 125 mil | Total |
3M 4508 Single-Coated Foam Tape 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast.. |
|||
Thickness | 3180 microns | 125 mil | Total |
3M 4718 Single-Coated Foam Tape 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast.. |
|||
Thickness | 3180 microns | 125 mil | |
3M Bumpon™ SJ5808 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Thickness | 3180 - 12700 microns | 125 - 500 mil | Range of Thicknesses Available |
Rogers Corporation Bisco® BF-2000 Ultra-Soft Silicone Foam BISCO® Ultra Soft is a highly compressible silicone foam. The combination of low weight and softness makes this flame retardant foam ideal for transportation, industrial and electronics applicatio.. |