Polymer Property : Thickness = 7.00 mil Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 127 - 178 microns
5.00 - 7.00 mil
Side 1
Arlon 19571R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place o..
Thickness 127 - 178 microns
5.00 - 7.00 mil
Side 2
Arlon 19571R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place o..
Thickness 152 - 178 microns
6.00 - 7.00 mil
with adhesive
3M Scotchcal™ 3662 Graphic Film
This is a 2-mil, durable, opaque film designed for making short term graphics that are applied to unsealed, outdoor, pedestrian traffic surfaces or selected smooth-to-rough wall surfaces. This film ..
Thickness 152 - 178 microns
6.00 - 7.00 mil
with adhesive
3M Scotchcal™ 8662 Graphic Film
This is a 2-mil, durable, opaque film designed for making short term graphics that are applied to unsealed, outdoor, pedestrian traffic surfaces or selected smooth-to-rough wall surfaces. This film ..