3M 9589 Double Coated Tapes with Adhesive 700 Series

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 9589 Double Coated Tapes with Adhesive 700 Series.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Double Coated Tapes with 3M™ Adhesive 700 Series feature a high tack synthetic rubber adhesive which provides excellent quick stick or initial adhesion and bonds together a wide variety of materials such as metals, papers, paints and most plastics. These tapes have a film carrier, which can add dimensional stability for aid in removal and also provides easier handling during slitting and die-cutting.Information provided by 3M
Physical Properties Metric English Comments
Thickness 76.2 microns
3.00 mil
Faceside Adhesive
76.2 microns
3.00 mil
Carrier
76.2 microns
3.00 mil
Backside Adhesive
102 microns
4.00 mil
Liner Caliper
229 microns
9.00 mil
Tape Caliper
Mechanical Properties Metric English Comments
Peel Strength 0.6793 kN/m
3.875 pli
to Polypropylene, 90°, 2 mil Al foil, 72 hr RT; ASTM D3330
0.88746 kN/m
5.0625 pli
to Stainless Steel, 90°, 2 mil Al foil, 15 min RT; ASTM D3330
0.8984 kN/m
5.125 pli
to Polyester, 90°, 2 mil Al foil, 72 hr RT; ASTM D3330
0.920 kN/m
5.25 pli
to Stainless Steel, 90°, 2 mil Al foil, 72 hr RT; ASTM D3330
0.95319 kN/m
5.4375 pli
to Stainless Steel, 90°, 2 mil Al foil, 72 hr at 70°C; ASTM D3330
1.1066 kN/m
6.3125 pli
to Polycarbonate, 90°, 2 mil Al foil, 72 hr RT; ASTM D3330
1.2819 kN/m
7.3125 pli
to Stainless Steel, 90°, 2 mil Al foil, 72 hr RT; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 49.0 °C
120 °F
Long term
70.0 °C
158 °F
Short term
Processing Properties Metric English Comments
Shelf Life 18.0 Month
18.0 Month
Descriptive Properties Value Comments
Appearance White
Liner Green plaid, 60# Densified Kraft