Polymer Property : Water Vapor Transmission = 10.9 g/m²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Water Vapor Transmission 10.9 g/m²/day

@Thickness 0.0254 mm
0.702 g/100 in²/day

@Thickness 0.00100 in
ASTM F1249
Total 9458 HDPE Film Grade
Medium molecular weight grade. Excellent bubble stability, good compatibility with LDPE and LLDPE, good heat resistance, high stiffness and tensile strength.Applications: Release liners, Stand-up ba..
Water Vapor Transmission 10.9 g/m²/day

@Temperature 37.8 °C
0.700 g/100 in²/day

@Temperature 100 °F
ASTM F1249
Total HDPE HL 535 High Density Polyethylene, Film Resin
Polyethylene: Medium molecular weight, high density film resinCharacteristics:High stiffnessGood heat resistanceExcellent bubble stabilityGood compatibility with LDPE and LLDPEApplications:Release ..
Water Vapor Transmission 10.9 g/m²/day

@Temperature 37.8 °C
0.700 g/100 in²/day

@Temperature 100 °F
90% RH; ASTM F1249-90
Total PPH 3575CC Polypropylene Homopolymer, Film Grade
Low Residuals TOTAL Polypropylene 3575CC utilizes the new TOTAL Polypropylene proprietary process technology to provide extremely low residuals for improved color stability and clarity.Slip/Antiblo..
Water Vapor Transmission 10.9 g/m²/day

@Temperature 37.8 °C
0.700 g/100 in²/day

@Temperature 100 °F
90% RH; ASTM F1249-90
Total PPR 6575 Polypropylene, Random Copolymer, Film Grade
Color. Low catalyst residuals in TOTAL Petrochemicals 6575 polypropylene results in improved color stability.Clarity/Impact. The random copolymer structure of 6575 improves its clarity and resilien..
Water Vapor Transmission 10.9 g/m²/day
0.702 g/100 in²/day
38°C, 90% RH; ExxonMobil Method
ExxonMobil Bicor® 50 LBW OPP Film
Product Description: Bicor LBW is a two-sided treated, slip modified, non-heat sealable OPP film designed for use as the outside web of a lamination. The print surface is treated and can be printed ..