Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 12.0 g/m²/day | 0.773 g/100 in²/day | |
LG Chemical LUTENE BB0808 LDPE Blown Film Grade Description: LUTENE BB0808 is mainly intended for the extrusion of blown film with high mechanical property for the manufacture of shrink film and pallet shrink covers. LUTENE BB0808 have the balanc.. |
|||
Water Vapor Transmission | 12.0 g/m²/day | 0.773 g/100 in²/day | |
LG Chemical LUTENE FB0800 LDPE Blown Film Description: LUTENE FB0800 is mainly intended for the extrusion of blown film with high mechanical property for the manufacture of greenhouse film. LUTENE FB0800 have the excellent mechanical proper.. |