Physical Properties Metric English Comments
Oxygen Transmission Rate 9.31 - 13.97 cc/m²/day
0.600 - 0.8997 cc/100 in²/day
77°F / 0% / RH; ASTM D3985
Honeywell Capran® Emblem™ 1230 Bi-Axially Oriented Nylon Film  (discontinued **)
Description: Capran® Emblem™ 1230 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbo..
Oxygen Transmission Rate 9.31 - 13.97 cc/m²/day
0.600 - 0.8997 cc/100 in²/day
77°F / 0% / RH; ASTM D3985
Honeywell Capran® Emblem™ 1530 PVDC-Coated Bi-Axially Oriented Nylon Film  (discontinued **)
Capran® Emblem™ 1530 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbons, and many ..
Oxygen Transmission Rate 7.76 - 13.97 cc/m²/day
0.500 - 0.8997 cc/100 in²/day
77°F / 0% / RH; ASTM D3985
Honeywell Capran® Emblem™ 2530 Bi-Axially Oriented Nylon Film  (discontinued **)
Description: Capran® Emblem™ 2530 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbo..