Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 11 g/10 min @Load 2.16 kg, Temperature 190 °C |
11 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Versollan™ OM 1262NX-1 Thermoplastic Elastomer (TPE) Versollan™ OM 1262NX-1 is a performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS and PC/ABS substrates. - Excellent Grip with Matte, Rubbery Finish - Proven Track R.. |
|||
Melt Flow | 11 g/10 min @Load 21.6 kg, Temperature 190 °C |
11 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
SABIC FI1157 Bimodal High Density Polyethylene for Blown Film Product Description: FI1157 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh.. |
|||
Melt Flow | 11 g/10 min @Load 5.00 kg, Temperature 260 °C |
11 g/10 min @Load 11.0 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycoloy® C4220K PC+ABS (Asia Pacific) Cycoloy* C4220K resin is an injection moldable 20% glass reinforced non FR PC-ABS.
Key features include improved Knit Line strength, good flow, excellent strength & rigidity, heat resistance & hyd.. |
|||
Melt Flow | 11 g/10 min @Load 5.00 kg, Temperature 260 °C |
11 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics GELOY CR8510 ASA (Asia Pacific) ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated. |
|||
Melt Flow | 11 g/10 min @Load 1.20 kg, Temperature 300 °C |
11 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele.. |
|||
Melt Flow | 11 g/10 min @Load 1.20 kg, Temperature 300 °C |
11 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® FXE144H PC (Asia Pacific) FXE144H is a Lexan PC Translucent Grade in our VisualFX Portfolio. It is part of Energy family, which includes Illuminate, Glass, and Flame effects. Grade was developed to meet the Aesthetic Differe.. |
|||
Melt Flow | 11 g/10 min @Load 1.20 kg, Temperature 300 °C |
11 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® FXE144H PC (Asia Pacific) FXE144H is a Lexan PC Translucent Grade in our VisualFX Portfolio. It is part of Energy family, which includes Illuminate, Glass, and Flame effects. Grade was developed to meet the Aesthetic Differe.. |
|||
Melt Flow | 11 g/10 min @Load 1.20 kg, Temperature 300 °C |
11 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® FXM141R PC FXM141R is a Lexan PC grade in Metallic or Pearlescent effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color .. |
|||
Melt Flow | 11 g/10 min @Load 10.0 kg, Temperature 220 °C |
11 g/10 min @Load 22.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Geloy XTWE280 ASA (Asia Pacific) Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 11 g/10 min @Load 10.0 kg, Temperature 230 °C |
11 g/10 min @Load 22.0 lb, Temperature 446 °F |
Rate; ASTM-D1238 |
Ineos ABS Lustran® 261 ABS, High-Impact Blending Grade Lustran® ABS 261 resin is a natural, stiffer-flow, virgin blending grade of ABS (acrylonitrile butadiene styrene). It is designed for use with other high-impact ABS resins for drain, waste, and v.. |
|||
Melt Flow | 11 g/10 min @Load 5.00 kg, Temperature 250 °C |
11 g/10 min @Load 11.0 lb, Temperature 482 °F |
ISO 1133 |
SABIC Innovative Plastics Valox® ENH8560 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 30% Glass fiber reinforced PBT/PET blend |
|||
Melt Flow | 11 g/10 min @Load 5.00 kg, Temperature 250 °C |
11 g/10 min @Load 11.0 lb, Temperature 482 °F |
ISO 1133 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Melt Flow | 11 g/10 min @Load 2.16 kg, Temperature 230 °C |
11 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Samyang Triel® 5450 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5450 is an extrusion grade.Information provided by Samyang. |
|||
Melt Flow | 11 g/10 min @Load 5.00 kg, Temperature 280 °C |
11 g/10 min @Load 11.0 lb, Temperature 536 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Noryl GTX GTX965 PPE+PA66 NORYL GTX965 is a mineral reinforced PPE/PA blend. It offers excellent surface appearance, processability and dimensional stability at elevated temperatures. The best molding condition for good appe.. |
|||
Melt Flow | 11 g/10 min @Load 5.00 kg, Temperature 280 °C |
11 g/10 min @Load 11.0 lb, Temperature 536 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 (Europe-Africa-Middle East) Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
Melt Flow | 11 g/10 min @Load 5.00 kg, Temperature 280 °C |
11 g/10 min @Load 11.0 lb, Temperature 536 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq.. |
|||
Melt Flow | 11 g/10 min @Load 5.00 kg, Temperature 220 °C |
11 g/10 min @Load 11.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem HU2410 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications.
Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
Melt Flow | 11 g/10 min @Load 5.00 kg, Temperature 266 °C |
11 g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D 1238 |
SABIC Innovative Plastics Xenoy® X5630 PC+PET Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applicationsThis data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 11 g/10 min @Load 2.16 kg, Temperature 265 °C |
11 g/10 min @Load 4.76 lb, Temperature 509 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Xylex X7529 PC+POLYESTER (Asia Pacific) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical quality. UV 400nm block.This data was supplied by SABIC-IP for the Asia Pacif.. |
|||
Melt Flow | 11 g/10 min @Load 2.16 kg, Temperature 265 °C |
11 g/10 min @Load 4.76 lb, Temperature 509 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Xylex X7529OQ PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical qualityThis data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
Melt Flow | 11 g/10 min @Load 5.00 kg, Temperature 280 °C |
11 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D 1238 |
SABIC Innovative Plastics Noryl GFN1420V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe.. |
|||
Melt Flow | 11 g/10 min @Load 21.6 kg, Temperature 190 °C |
11 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® FB 75 HDPE Made for tubular film applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 11 g/10 min @Load 2.16 kg, Temperature 230 °C |
11 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Daplen™ EE188AI Polypropylene TPO Compound Daplen™ EE188AI is a 15% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. .. |
|||
Melt Flow | 11 g/10 min @Load 2.16 kg, Temperature 230 °C |
11 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Daplen™ EE189AI Polypropylene TPO Compound Daplen™ EE189AI is a 15% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. .. |
|||
Melt Flow | 11 g/10 min @Load 2.16 kg, Temperature 230 °C |
11 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Daplen™ SB4411/2 Polypropylene Compound Elastomer and Mineral Modified Daplen SB4411/2 is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. The product is available in black, but other colors can be provided on request.Daplen .. |
|||
Melt Flow | 11 g/10 min @Load 2.16 kg, Temperature 260 °C |
11 g/10 min @Load 4.76 lb, Temperature 500 °F |
ISO 1133 |
Topas Advanced Polymers TOPAS® Elastomer E-140 Developmental Cyclic Olefin Copolymer (COC) TOPAS® Elastomer E-140, unlike most TOPAS grades, is a semicrystalline cyclic olefin material with flexibility. It is a fairly stiff elastomer which can be extruded and injection molded, and can be.. |
|||
Melt Flow | 11 g/10 min @Load 3.80 kg, Temperature 230 °C |
11 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Diamond Polymers ABS 2100 P Compounding Grade Powder Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 11 g/10 min @Load 1.20 kg, Temperature 300 °C |
11 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® FXE144H PC (Europe-Africa-Middle East) FXE144H is a Lexan PC Translucent Grade in our VisualFX Portfolio. It is part of Energy family, which includes Illuminate, Glass, and Flame effects. Grade was developed to meet the Aesthetic Differe.. |
|||
Melt Flow | 11 g/10 min @Load 2.16 kg, Temperature 265 °C |
11 g/10 min @Load 4.76 lb, Temperature 509 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Xylex X7529OQ PC+POLYESTER (Asia Pacific) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical qualityThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 11 g/10 min @Load 10.0 kg, Temperature 190 °C |
11 g/10 min @Load 22.0 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Paxon™ 4700 Blown Film Extrusion Resin
(discontinued **) 4700 is a medium molecular weight, high density polyethylene homopolymer film resin. It can be processed on conventional film extrusion equipment.Information provided by ExxonMobil Chemical |