Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.3 g/10 min @Load 5.00 kg, Temperature 230 °C |
2.3 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
DuPont Performance Polymers Hytrel® HTR8223 BK320 TPC-ET
(Unverified Data**) Hytrel® HTR8223 BK320 is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal hardness of 42D, is pigmented black with fine particle size carbon black, a.. |
|||
Melt Flow | 2.3 g/10 min @Load 10.0 kg, Temperature 220 °C |
2.3 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Techmer ES Plastiblend® ABS 8006 Availability: North AmericaForms: PelletsProcessing Method: Sheet ExtrusionInformation provided by TP Composites, Inc. |
|||
Melt Flow | 2.3 g/10 min @Load 10.0 kg, Temperature 220 °C |
2.3 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Techmer ES Plastiblend® ABS 8010 Availability: North AmericaForms: PelletsProcessing Method: Extrusion Blow Molding and Sheet ExtrusionInformation provided by TP Composites, Inc. |
|||
Melt Flow | 2.3 g/10 min @Load 5.00 kg, Temperature 190 °C |
2.3 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Borealis BB125MO Polypropylene Copolymer BB125MO is a heterophasic copolymer. This grade is a low melt flow rate grade intended for blow molding and sheet extrusion, and features extremely good process ability with improved melt strength a.. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 100STE NC010 Acetal (POM)
(Unverified Data**) Super Toughened High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100STE NC010 (formerly DE20590) is a high-viscosity super-toughened acetal homopolymer with very low VOC emissions. P.. |
|||
Melt Flow | 2.3 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.3 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 3500ELG Description: Injection Molding Grade, Medium Impact, Low GlossInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 2.3 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.3 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 3502ELG Description: Injection Molding Grade, Medium Impact, Low GlossInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 100 NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |