Material Notes:
Availability: North AmericaForms: PelletsProcessing Method: Sheet ExtrusionInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
ASTM D792
Melt Flow 0.20 g/10 min

@Load 3.80 kg,
Temperature 230 °C
0.20 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
2.3 g/10 min

@Load 10.0 kg,
Temperature 220 °C
2.3 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Elongation at Break 3.4 %
3.4 %
ASTM D638
Flexural Strength 58.6 MPa
8500 psi
ASTM D790
Flexural Modulus 1.93 GPa
280 ksi
ASTM D790
Izod Impact, Notched 1.71 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
3.20 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
4.00 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
7.50 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 95.0 °C
203 °F
Deflection Temperature at 0.46 MPa (66 psi) 79.4 °C
175 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 93.9 °C
201 °F
Unannealed; ASTM D648