Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 22 g/10 min @Load 2.16 kg, Temperature 190 °C |
22 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Versaflex™ OM 9-801N Thermoplastic Elastomer (TPE) Versaflex™ OM 9-801N is designed for overmolding onto a wide variety of substrates including PC, ABS, PC/ABS, HIPS, PPO, acetal, acrylic and copolyester. - Bonds to a Variety Of Substrates - Rubber.. |
|||
Melt Flow | 22 g/10 min @Load 2.16 kg, Temperature 190 °C |
22 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Versalloy™ XL 9055X-9 Thermoplastic Elastomer (TPE) Versalloy™ XL 9055X-9 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Overmold Adhesion to Polypro.. |
|||
Melt Flow | 22 g/10 min @Load 5.00 kg, Temperature 260 °C |
22 g/10 min @Load 11.0 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS (Europe-Africa-Middle East) High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra.. |
|||
Melt Flow | 22 g/10 min @Load 5.00 kg, Temperature 260 °C |
22 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D 1238 |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Europe-Africa-Middle East) CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of propertiesThis data was supplied by.. |
|||
Melt Flow | 22 g/10 min @Load 2.16 kg, Temperature 260 °C |
22 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D 1238 |
SABIC Innovative Plastics Cycoloy® CX7110 PC+ABS (Europe-Africa-Middle East) Cycoloy* resin grade CX7110 is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant systems. Excellent impact/flow balance together with a UL-94 V0 rating at 1... |
|||
Melt Flow | 22 - 28 g/10 min @Load 2.16 kg, Temperature 190 °C |
22 - 28 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4020W (20425) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 22 - 28 g/10 min @Load 2.16 kg, Temperature 190 °C |
22 - 28 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4025W (25425) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 22 g/10 min @Load 3.80 kg, Temperature 230 °C |
22 g/10 min @Load 8.38 lb, Temperature 446 °F |
Cond I; ASTM D1238 |
Ravago Manufacturing Americas Hylac® HF224 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Melt Flow | 22 g/10 min @Load 5.00 kg, Temperature 260 °C |
22 g/10 min @Load 11.0 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra.. |
|||
Melt Flow | 22 g/10 min @Load 21.6 kg, Temperature 190 °C |
22 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) EX 1 HF 7740F2 High Density Polyethylene EX1 (HF 7740F2) is high density polyethylene with Butene-1 as co monomer. It is a medium molecular mass with a narrow molar mass distribution.Application: stretched film tape used in manufacture o.. |
|||
Melt Flow | 22 g/10 min @Load 10.0 kg, Temperature 200 °C |
22 g/10 min @Load 22.0 lb, Temperature 392 °F |
ISO 1133 |
Kuraray SEPTON® S2104 Thermoplastic Rubber SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi.. |
|||
Melt Flow | 22 g/10 min @Load 10.0 kg, Temperature 220 °C |
22 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
MBA Polymers ABS 4124 Recycled acrylonitrile-butadiene-styrene copolymer Available in standard black.Information provided by MBA Polymers. |
|||
Melt Flow | 22 g/10 min @Load 1.20 kg, Temperature 300 °C |
22 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics PC2200 PC (Asia Pacific) PC2200 resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.. |
|||
Melt Flow | 22 g/10 min @Load 1.20 kg, Temperature 300 °C |
22 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics PC2200 PC (Europe-Africa-Middle East) PC2200 resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.. |
|||
Melt Flow | 22 g/10 min @Load 1.20 kg, Temperature 300 °C |
22 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics PC2200R PC (Europe-Africa-Middle East) PC2200R resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplied by S.. |
|||
Melt Flow | 22 g/10 min @Load 1.20 kg, Temperature 300 °C |
22 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics PC2203R PC PC2203R resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was suppli.. |
|||
Melt Flow | 22 g/10 min @Load 5.00 kg, Temperature 360 °C |
22 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem ATX202R PEI+PCE 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 22 g/10 min @Load 5.00 kg, Temperature 360 °C |
22 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Melt Flow | 22 g/10 min @Load 6.60 kg, Temperature 337 °C |
22 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem ATX203R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 22 g/10 min @Load 6.60 kg, Temperature 337 °C |
22 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem ATX203R PEI+PCE (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 22 g/10 min @Load 6.60 kg, Temperature 337 °C |
22 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem ATX203R PEI+PCE (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Melt Flow | 22 g/10 min @Load 10.0 kg, Temperature 250 °C |
22 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® CF-1051 PC, Unreinforced High Impact High-impact material for the exterior material of mobile phoneInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 22 g/10 min @Load 5.00 kg, Temperature 220 °C |
22 g/10 min @Load 11.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 (Asia Pacific) High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 22 g/10 min @Load 5.00 kg, Temperature 220 °C |
22 g/10 min @Load 11.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 (Europe-Africa-Middle East) High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 22 g/10 min @Load 2.16 kg, Temperature 230 °C |
22 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Xmod™ BG055AI High Stiffness Polypropylene for Injection Molding Applications Xmod BG055AI is a high melt flow polypropylene with increased crystallinity, intended for injection molding. Xmod BG055AI is a very easy flowing material with a good balance between impact strength.. |
|||
Melt Flow | 22 g/10 min @Load 2.16 kg, Temperature 190 °C |
22 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® FB/FL 20 HDPE Made for tubular film and special applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 22 g/10 min @Load 21.6 kg, Temperature 190 °C |
22 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Total HDPE 5802 High Density Polyethylene - Blow Molding HDPE 5802 is a high density polyethylene with excellent compromise between stiffness and Environmental Stress Crack Resistance. It has been specifically designed for the manufacture of blow molded .. |
|||
Melt Flow | 22 g/10 min @Load 10.0 kg, Temperature 265 °C |
22 g/10 min @Load 22.0 lb, Temperature 509 °F |
ISO 1133 |
Denka MALECCA K-400 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Melt Flow | 22 g/10 min @Load 10.0 kg, Temperature 220 °C |
22 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO-1133 |
Chi Mei Polylac® PA-757 ABS High gloss, medium impact |
|||
Melt Flow | 22 g/10 min @Load 10.0 kg, Temperature 230 °C |
22 g/10 min @Load 22.0 lb, Temperature 446 °F |
ASTM D1238 |
ExxonMobil EXXELOR™ VA 1803 Maleic anhydride functionalized elastomeric ethylene copolymer Product Description: Exxelor VA 1803 polymer resin is a high flow, amorphous ethylene copolymer functionalized with maleic anhydride by reactive extrusion. Its fully saturated backbone results in ou.. |