Polymer Property : Melt Flow = 7.7 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 7.7 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.7 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
PolyOne Versaflex™ 9570-1 Thermoplastic Elastomer (TPE)
Versaflex™ 9570-1 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to ..
Melt Flow 7.7 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.7 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
PolyOne Versaflex™ 9570-9 Thermoplastic Elastomer (TPE)
Versaflex™ 9570-9 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to ..
Melt Flow 7.7 g/10 min

@Load 2.16 kg,
Temperature 220 °C
7.7 g/10 min

@Load 4.76 lb,
Temperature 428 °F
cm³/10min; ISO 1133
DuPont Performance Polymers Hytrel® 4069 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Melt Flow 7.7 g/10 min

@Load 1.00 kg,
Temperature 235 °C
7.7 g/10 min

@Load 2.20 lb,
Temperature 455 °F
ASTM D1238
Diamond Polymers Softflex® SF 5560 Overmold for Nylon
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Melt Flow 7.7 g/10 min

@Load 1.00 kg,
Temperature 235 °C
7.7 g/10 min

@Load 2.20 lb,
Temperature 455 °F
ASTM D1238
Diamond Polymers Softflex® 1701-1402
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.