Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 7.7 g/10 min @Load 2.16 kg, Temperature 190 °C |
7.7 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Versaflex™ 9570-1 Thermoplastic Elastomer (TPE) Versaflex™ 9570-1 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to .. |
|||
Melt Flow | 7.7 g/10 min @Load 2.16 kg, Temperature 190 °C |
7.7 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Versaflex™ 9570-9 Thermoplastic Elastomer (TPE) Versaflex™ 9570-9 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to .. |
|||
Melt Flow | 7.7 g/10 min @Load 2.16 kg, Temperature 220 °C |
7.7 g/10 min @Load 4.76 lb, Temperature 428 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Hytrel® 4069 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Melt Flow | 7.7 g/10 min @Load 1.00 kg, Temperature 235 °C |
7.7 g/10 min @Load 2.20 lb, Temperature 455 °F |
ASTM D1238 |
Diamond Polymers Softflex® SF 5560 Overmold for Nylon Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 7.7 g/10 min @Load 1.00 kg, Temperature 235 °C |
7.7 g/10 min @Load 2.20 lb, Temperature 455 °F |
ASTM D1238 |
Diamond Polymers Softflex® 1701-1402 Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |