Physical Properties Metric English Comments
Oxygen Transmission 236 cc-mm/m²-24hr-atm
599 cc-mil/100 in²-24hr-atm
or 14100 cc/m²-24hr-atm for the 50 gauge film. ASTM D3985
DuPont™ Clysar® VHP Polyolefin Shrink Packaging Film, 50 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.DuPont Clysar® VHP is a thin gauge, clear, biaxially oriented, heat shrinkable polyolefin film. It provides strong seals and excellent optics under a wide..
Oxygen Transmission 236 cc-mm/m²-24hr-atm
599 cc-mil/100 in²-24hr-atm
or 6200 cc/m²-24hr-atm for the film. ASTM D3985
DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 38.1 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, e..
Oxygen Transmission 236 cc-mm/m²-24hr-atm
599 cc-mil/100 in²-24hr-atm
or 3100 cc/m²-24hr-atm for the film. ASTM D3985
DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 76.2 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, e..
Oxygen Transmission 236 cc-mm/m²-24hr-atm
599 cc-mil/100 in²-24hr-atm
or 3100 cc/m²-24hr-atm for the film. ASTM D3985
DuPont™ Sclairfilm® LX-3 LLDPE Film, Laminating, 76.2 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, e..
Oxygen Transmission 236 cc-mm/m²-24hr-atm
599 cc-mil/100 in²-24hr-atm
or 6200 cc/m²-24hr-atm for the film. ASTM D3985
DuPont™ Sclairfilm® GL-1 LLDPE Film, Laminating, 38.1 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an..
Oxygen Transmission 236 cc-mm/m²-24hr-atm
599 cc-mil/100 in²-24hr-atm
or 3100 cc/m²-24hr-atm for the film. ASTM D3985
DuPont™ Sclairfilm® GL-1 LLDPE Film, Laminating, 76 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an..
Oxygen Transmission 236 cc-mm/m²-24hr-atm
599 cc-mil/100 in²-24hr-atm
or 6200 cc/m²-24hr-atm for the film. ASTM D3985
DuPont™ Sclairfilm® GL-3 LLDPE Film, Laminating, 38.1 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an..
Oxygen Transmission 236 cc-mm/m²-24hr-atm
599 cc-mil/100 in²-24hr-atm
or 3100 cc/m²-24hr-atm for the film. ASTM D3985
DuPont™ Sclairfilm® GL-3 LLDPE Film, Laminating, 76 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an..
Oxygen Transmission 236 cc-mm/m²-24hr-atm
599 cc-mil/100 in²-24hr-atm
or 3100 cc/m²-24hr-atm for the film. ASTM D3985
DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 76.2 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st..
Oxygen Transmission 236 cc-mm/m²-24hr-atm
599 cc-mil/100 in²-24hr-atm
or 3100 cc/m²-24hr-atm for the film. ASTM D3985
DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 76.2 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st..
Oxygen Transmission 236 cc-mm/m²-24hr-atm
599 cc-mil/100 in²-24hr-atm
or 6200 cc/m²-24hr-atm for the film. ASTM D3985
DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 38.1 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st..
Oxygen Transmission 236 cc-mm/m²-24hr-atm
599 cc-mil/100 in²-24hr-atm
or 6200 cc/m²-24hr-atm for the film. ASTM D3985
DuPont™ Sclairfilm® LX-3 LLDPE Film, Laminating, 38.1 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, e..
Oxygen Transmission 236 cc-mm/m²-24hr-atm
599 cc-mil/100 in²-24hr-atm
or 6200 cc/m²-24hr-atm for the film. ASTM D3985
DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 38.1 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st..