Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont™ Sclairfilm® GL-3 LLDPE Film, Laminating, 76 µm Thickness  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Sclairfilm® GL-3 LLDPE Film, Laminating, 76 µm Thickness  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal and hot tack characteristics along with good physical strength and opticals.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
Moisture Vapor Transmission 0.360 cc-mm/m²-24hr-atm
0.914 cc-mil/100 in²-24hr-atm
ASTM E96 Procedure E
Water Vapor Transmission 4.70 g/m²/day
0.303 g/100 in²/day
ASTM E96 Procedure E
Oxygen Transmission 236 cc-mm/m²-24hr-atm
599 cc-mil/100 in²-24hr-atm
or 3100 cc/m²-24hr-atm for the film. ASTM D3985
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 600 %
600 %
ASTM D882
Tensile Modulus 0.190 GPa
27.6 ksi
ASTM D882
Dart Drop Test 170 g
0.375 lb
Film Tensile Strength at Break, MD 32.0 MPa
4640 psi
ASTM D882
Optical Properties Metric English Comments
Haze 12 %
12 %
ASTM D1003
Gloss 80 %
80 %
20°; ASTM D2457
Users viewing this material also viewed the following: