Environmental Stress Crack Resistance 2.00 - 1500 hour
2.00 - 1500 hour
Average value: 770 hour Grade Count:7
Overview of materials for High Density Polyethylene (HDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max..
Environmental Stress Crack Resistance 30.0 - 1500 hour
30.0 - 1500 hour
Average value: 671 hour Grade Count:9
Overview of materials for High Density Polyethylene (HDPE), Sheet/Thermoforming Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Sheet/Thermoforming Grade". Each property range of values reported is ..
Environmental Stress Crack Resistance 1.00 - 1500 hour
1.00 - 1500 hour
Average value: 338 hour Grade Count:6
Overview of materials for Low Density Polyethylene (LDPE), Molded