Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | 30.0 - 5000 hour | 30.0 - 5000 hour | Average value: 1220 hour Grade Count:6 |
Overview of materials for Medium Density Polyethylene (MDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Molded". Each property range of values reported is minimum and maxim.. |
|||
Environmental Stress Crack Resistance | 30.0 - 1500 hour | 30.0 - 1500 hour | Average value: 671 hour Grade Count:9 |
Overview of materials for High Density Polyethylene (HDPE), Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Sheet/Thermoforming Grade". Each property range of values reported is .. |