Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | 30 hour | 30 hour | F50, Condition A, ASTM D1693, 100% Igepal |
NOVA Chemicals Sclair® 2508-UV9 MDPE Injection Molding Resin
(discontinued **) Features: Excellent processability for applications requiring stiffness and toughness, good cold temperature impact properties.Applications: Roll-out cart lids.Data provided by the manufacturer. |
|||
Environmental Stress Crack Resistance | >= 30 hour | >= 30 hour | |
Kazanorgsintez PE2NT21-13 High Density Polyethylene Composite Production Method: Copolymerization of eythylene at low pressure in presence of complex catalysts using gaseous-phase method. Application: Composition is intended for injection molding processin.. |
|||
Environmental Stress Crack Resistance | >= 30 hour | >= 30 hour | |
Kazanorgsintez PE2NT74-15 High Density Polyethylene for Blow Molding Production Method: Gaseous-phase method. Application: Compositions are intended for goods produced by injection molding method.Information Provided by Kazanorgsintez |
|||
Environmental Stress Crack Resistance | >= 30 hour | >= 30 hour | |
Kazanorgsintez PE2NT75-15 High Density Polyethylene for Blow Molding Production Method: Gaseous-phase method. Application: Compositions are intended for goods produced by injection molding method.Information Provided by Kazanorgsintez |
|||
Environmental Stress Crack Resistance | >= 30 hour | >= 30 hour | |
Kazanorgsintez PE2NT76-17 High Density Polyethylene for Blow Molding Production Method: Gaseous-phase method. Application: Compositions are intended for goods produced by injection molding method.Information Provided by Kazanorgsintez |
|||
Environmental Stress Crack Resistance | 30 hour | 30 hour | F<sub>50</sub>; ASTM D1693 |
LyondellBasell Petrothene® LR732001 High Density Polyethylene (Blow Molding Grade) ApplicationsThe PETROTHENE LR 7320 series of polyethylene resins exhibits an excellent balance of stiffness and environmental stress crack resistance. Typical applications include bottles for bleac.. |
|||
Environmental Stress Crack Resistance | 30 hour | 30 hour | F<sub>50</sub>; ASTM D1693 |
LyondellBasell Petrothene® LR732001 High Density Polyethylene (Sheet & Profile Grade) ApplicationsThe PETROTHENE LR 7320 series of polyethylene resins exhibits an excellent balance of stiffness and environmental stress crack resistance. Regulatory StatusThe base resin LR 7320 meets t.. |
|||
Environmental Stress Crack Resistance | 30 hour | 30 hour | F<sub>50</sub>; ASTM D1693 |
LyondellBasell Petrothene® LR732011 High Density Polyethylene (Blow Molding Grade) ApplicationsThe PETROTHENE LR 7320 series of polyethylene resins exhibits an excellent balance of stiffness and environmental stress crack resistance. Typical applications include bottles for bleac.. |
|||
Environmental Stress Crack Resistance | 30 hour | 30 hour | F<sub>50</sub>; ASTM D1693 |
LyondellBasell Petrothene® LR732013 High Density Polyethylene (Blow Molding Grade) ApplicationsThe PETROTHENE LR 7320 series of polyethylene resins exhibits an excellent balance of stiffness and environmental stress crack resistance. Typical applications include bottles for bleac.. |
|||
Environmental Stress Crack Resistance | 30 hour | 30 hour | F<sub>50</sub>; ASTM D1693 |
LyondellBasell Petrothene® LR732031 High Density Polyethylene ApplicationsPETROTHENE LR 7320-31 is a high density polyethylene resin that exhibits an excellent balance of stiffness and environmental stress crack resistance. This resin has outstanding extrusio.. |
|||
Environmental Stress Crack Resistance | >= 30 hour | >= 30 hour | F50; ASTM D1693 |
LG Chemical SEETEC PB270 HDPE Features: This high molecular weight, hexane copolymer is tailored for light-weight blow-molded containers that require: Good stiffness and Excellent processabilityAdditives: Anti-OxidantsApplicatio.. |
|||
Environmental Stress Crack Resistance | 30 hour | 30 hour | F<sub>50</sub>; ASTM D1693 |
Lotte Chemical Titan TITANZEX® HM5000 High density polyethylene HM5000 is a high density polyethylene for extrusion monofilament. HM5000 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3... |
|||
Environmental Stress Crack Resistance | 30 hour | 30 hour | ASTM D1693 |
Global S-5000 High Density Polyethylene Description-good for monofilament Applications-ropes, fishing net, agricultural net and sports netInformation provided by Global Polymers Corporation. |
|||
Environmental Stress Crack Resistance | 30 hour | 30 hour | ASTM D1894 |
Iran Petrochemical (PCC) 5030UA High Density Polyethylene HD-5030UA is a high-density polyethylene copolymer grade with a narrow molecular weight distribution, specially developed for injection molding application requiring very high environmental stress c.. |
|||
Environmental Stress Crack Resistance | 30 hour @Temperature 50.0 °C |
30 hour @Temperature 122 °F |
F50, 25% Igepal; ASTM D1693 |
SCG Chemicals EL-Leneâ„¢ H5480S High Density Polyethylene Monofilament Key Characteristics:High tenacityExcellent product colorRecommended Applications: Monofilament and flat yarn extrusion for manufacturing of nets, ropes and tarpaulinInformation provided by SCG Chem.. |
|||
Environmental Stress Crack Resistance | 30 hour | 30 hour | Condition B, 10%; ASTM D1693 |
ExxonMobil LL 6201.19 Injection Molding Resin Product Description: LL 6201 is a narrow molecular weight butane copolymer designed for applications that require excellent toughness. This resin offers easy processability for applications that req.. |
|||
Environmental Stress Crack Resistance | 30 hour | 30 hour | F<sub>50</sub>; Condition A, 100% Igepal; ASTM D1693 |
NOVA Chemicals Sclair® 2508-UV13 MDPE Injection Molding Resin
(discontinued **) Excellent processability for applications requiring stiffness and toughness, Good cold temperature impact propertiesApplications: Roll-out cart lidsAdditives: Elevated levels of ultraviolet light st.. |