NOVA Chemicals Sclair® 2508-UV13 MDPE Injection Molding Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Sclair® 2508-UV13 MDPE Injection Molding Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent processability for applications requiring stiffness and toughness, Good cold temperature impact propertiesApplications: Roll-out cart lidsAdditives: Elevated levels of ultraviolet light stabilizers, Elevated levels of antioxidantsInformation provided by NOVA Chemicals.
Physical Properties Metric English Comments
Density 0.941 g/cc
0.0340 lb/in³
ASTM D792
Environmental Stress Crack Resistance 30 hour
30 hour
F<sub>50</sub>; Condition A, 100% Igepal; ASTM D1693
Melt Flow 11 g/10 min

@Load 2.16 kg,
Temperature 190 °C
11 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 63
63
ASTM D2240
Tensile Strength, Yield 19.0 MPa
2760 psi
50 mm/min; ASTM D638
Elongation at Break 400 %
400 %
50 mm/min; ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 119 °C
246 °F
ASTM D1525
Processing Properties Metric English Comments
Melt Temperature 170 - 215 °C
338 - 419 °F