Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 100000 - 150000 cP @Temperature 25.0 °C |
100000 - 150000 cP @Temperature 77.0 °F |
RVT, Spindle #7 @ 20rpm |
Lord Adhesives 6100 Silver Conductor LORD 6100 silver conductor is a one-component, thermosetting conductive epoxy designed primarily for surface mount attachment of electronic component devices. It is recommended for die attach and di.. |
|||
Brookfield Viscosity | 100000 cP | 100000 cP | 2HB CP52 Spindle @ 4.6rpm |
Lord Adhesives CircuitSAFâ„¢ MA-420 Epoxy Surface Mount Adhesive CircuitSAFâ„¢ MA-420 is an epoxy surface mount adhesive that cures rapidly at elevated temperatures and has been designed for use in high speed printed circuit board assembly for the attachment o.. |
|||
Brookfield Viscosity | 100000 - 120000 cP @Temperature 25.0 °C |
100000 - 120000 cP @Temperature 77.0 °F |
RVT, Spindle #7 @ 20rpm |
Lord Adhesives Metech 3288 Silver Conductor This product is a silver paste composition designed for screen print application of a solderable electrode base onto various types of electrical ceramic component devices. The fired film forms a hig.. |
|||
Brookfield Viscosity | 100000 - 400000 cP | 100000 - 400000 cP | Base, RVF #6 sp @ 2 rpm |
3M AC-250 A-1/6 Aerospace Sealant 3M Aerospace Sealant AC-250 A-1/6 is a two-part, low temperature curing polysulfide, quick repair sealant for integral fuel tank and fuselage sealing applications. The mixed compound is a pourable l.. |