Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 100000 - 150000 cP @Temperature 25.0 °C |
100000 - 150000 cP @Temperature 77.0 °F |
RVT, Spindle #7 @ 20rpm |
Lord Adhesives 6100 Silver Conductor LORD 6100 silver conductor is a one-component, thermosetting conductive epoxy designed primarily for surface mount attachment of electronic component devices. It is recommended for die attach and di.. |
|||
Brookfield Viscosity | 90000 - 150000 cP | 90000 - 150000 cP | Base, RVF #6 spindle, 20 rpm @ 27°C |
3M Scotch-Weld™ DP-100NS Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP-100NS is a two-part adhesives offering fast cure and machinability.Information provided by 3M |
|||
Brookfield Viscosity | 75000 - 150000 cP | 75000 - 150000 cP | Base, RFV #7 at 20 rpm |
3M Scotch-Weld™ DP190 Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Gray is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Gray and exhibits good peel, shear and environmental aging properties.Information pro.. |
|||
Brookfield Viscosity | 75000 - 150000 cP | 75000 - 150000 cP | Base, RVF #7 spindle, 20 rpm |
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |
|||
Brookfield Viscosity | 75000 - 150000 cP | 75000 - 150000 cP | Base, RVF #7 spindle, 20 rpm |
3M Scotch-Weld™ 2216 B/A Tan NS Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |