Physical Properties Metric English Comments
Brookfield Viscosity 200 - 400 cP

@Temperature 20.0 °C
200 - 400 cP

@Temperature 68.0 °F
Brookfield RVF sp. 2, 20 rpm solution at 15% in MEK; MQSA N0 40A
Lubrizol Advanced Materials Pearlstick® 45-50/03 Linear Thermoplastic Polyurethane Elastomer  (discontinued **
Pearlstick 45-50/03 is an elastic, linear, aromatic polyurethane with an extremely high crystallization rate and a medium-low thermoplasticity level, available as pellets.Solubility: Pearlstick 45-..
Brookfield Viscosity 200 - 400 cP

@Temperature 20.0 °C
200 - 400 cP

@Temperature 68.0 °F
Brookfield RVF sp. 3, 20 rpm solution at 15% in MEK; MQSA N° 40A
Lubrizol Advanced Materials Pearlstick® 49-46/03 Linear Thermoplastic Polyurethane Elastomer  (discontinued **
Pearlstick 49-46/03 is an elastic, linear, aromatic polyurethane with a very high crystallization rate and a low thermoplasticity level, available as pellets.Solubility: Pearlstick 49-46/03 is solu..
Brookfield Viscosity 25 - 400 cP
25 - 400 cP
#2/20 rpm
Mallard Creek Polymers ROVENE® 4041 SBR Latex
ROVENE® 4041 is a freeze-thaw stable carboxylated styrene-butadiene emulsion that can be used as a modifier for concrete applications. Concrete modified with ROVENE® 4041 is much tougher, more..
Brookfield Viscosity 50 - 400 cP
50 - 400 cP
#2/20 rpm
Mallard Creek Polymers ROVENE® 4176 SBR Latex
ROVENE® 4176 is a medium-soft carboxylated styrene-butadiene (SBR) latex emulsion. Its styrene content (50%) permits its use in formulating carpet laminating adhesives and flooring mastics. This ..
Brookfield Viscosity 50 - 400 cP
50 - 400 cP
Spindle # 2, rpm 60
Michelman® Michem® Flex P1883 Water based heat seal coating and primer
Description: Water based heat seal coating and primer for extrusion coated resins.Usage: Michem® Flex P1883 is a general purpose primer for metal and paper substrates to promote adhesion to extru..
Brookfield Viscosity 150 - 400 cP

@Temperature 25.0 °C
150 - 400 cP

@Temperature 77.0 °F
LVT, Spindle #3 @ 30rpm
Lord Adhesives Flocklok® 853 Blocked Flock Adhesive
Flocklok® 853 is a blocked, heat-curing, single coat adhesive used to adhere polyester or nylon fibers (flock) to a variety of elastomers including EPDM, NR, CR, and SBR. Flocked substrates provi..
Brookfield Viscosity 50 - 400 cP
50 - 400 cP
Spindle # 2, rpm 60
Michelman® Michem® Prime 4983R Ethylene acrylic acid dispersion
Description: Ethylene acrylic acid dispersionUsage: Michem® Prime 4983R provides outstanding adhesion to both metallic and cellulosic substrates, and enhances the water, grease, oil and solvent r..
Brookfield Viscosity 150 - 400 cP
150 - 400 cP
Spindle # 3, rpm 60
Michelman® VaporBase™ 1065 MVTR primer
Description: MVTR primerUsage: VaporBase™ 1065 is a primer designed to be used in tandem with the VaporCoat® series of products. VaporBase™ 1065 works to seal the base substrate allowin..
Brookfield Viscosity 150 - 400 cP
150 - 400 cP
Spindle # 3, rpm 60
Michelman® VaporBase™ 1075 Water resistance primer
Description: Water resistance primerUsage: VaporBase™ 1075 is a primer designed to be used in tandem with the VaporCoat® series of products as well as others. VaporBase™ 1075 works to s..
Brookfield Viscosity 100 - 400 cP
100 - 400 cP
Spindle # 2, rpm 60
Michelman® VaporCoat® 1500
Description: Water, oil and moisture resistant product for paperUsage: VaporCoat® 1500 is a coating which provides excellent water, oil and grease resistance along with excellent MVTR properties...
Brookfield Viscosity 200 - 400 cP
200 - 400 cP
Brookfield RVF sp 2, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A
Lubrizol Advanced Materials Pearlstick® 45-60/03 Polycaprolactone based TPU
Pearlstick 45-60/03 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with an extremely high crystallization rate and a medium thermoplasticity level.Solu..
Brookfield Viscosity 200 - 400 cP

@Temperature 20.0 °C
200 - 400 cP

@Temperature 68.0 °F
Brookfield RVF sp. 3, 20 rpm solution at 15% in MEK; MQSA N0 40A
Lubrizol Advanced Materials Pearlstick® 48-60/03 Linear Thermoplastic Polyurethane Elastomer
Pearlstick 48-60/03 is an elastic, linear, aromatic polyurethane with a very high crystallization rate and a low-medium thermoplasticity level, available as pellets.Solubility: Pearlstick 48-60..
Brookfield Viscosity 300 - 400 cP

@Temperature 25.0 °C
300 - 400 cP

@Temperature 77.0 °F
C.O.I.M. EXTER S® S 103 L Orthophthalic Resin
Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 103 L: Light-stabili..
Brookfield Viscosity 200 - 400 cP
200 - 400 cP
LVF Spindle #2 @ 30 rpm
3M Scotch-Weld™ FLX300 Flexible Instant Adhesive
3M™ Scotch-Weld™ Flexible Instant Adhesive FLX (formerly PR851) is formulated for extended resistance to impact, vibration, stress, peel, and humidity applications. It is faster curing than 3M™ S..
Brookfield Viscosity 200 - 400 cP
200 - 400 cP
LVF, sp 2 @ 30 rpm
3M Scotch-Weld™ MG300 FLX Medical Grade Instant Adhesive
3M™ Scotch-Weld™ Medical Grade Instant Adhesive are intended for use on a wide variety of materials used in the construction of disposable medical assemblies. They will quickly bond metals, plasti..
Brookfield Viscosity 100 - 400 cP
100 - 400 cP
RVT (15% in MEK); MQSA 40 A
Lubrizol Advanced Materials PEARLBOND® 151 Linear Thermoplastic Polyurethane  (discontinued **)
PEARLBOND® 125/H is polycaprolactone-based thermoplastic polyurethane, supplied in form of colourless or slightly yellowish, translucid pellets, combining a low hardness with excellent low-temperat..
Brookfield Viscosity 200 - 400 cP

@Temperature 23.9 °C
200 - 400 cP

@Temperature 75.0 °F
Mixed; ASTM D2393
BCC Products BC 8086 Urethane Casting
BC 8086 is a rapid setting, low viscosity, polyurethane casting system. It exhibits a working life of 45 seconds and obtains a demoldable hardness at 7 - 10 minutes. Some of the features include: no..