Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 130 cm³/g | 130 cm³/g | Viscosity number; ISO 307, 1157, 1628 |
Lanxess Pocan® B 7425 000000 PBT, 20% Glass Spheres PBT, 20% glass spheres, injection molding, low tendency to warp, improved surface finish |
|||
Viscosity Test | 130 cm³/g | 130 cm³/g | ISO 307 1157 1628 |
DuPont Performance Polymers Crastin® 6130 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin 6130 NC010 is an unreinforced medium high viscosity polybutylene terephthalate resin for .. |
|||
Viscosity Test | 130 cm³/g | 130 cm³/g | ISO 307 1157 1628 |
DuPont Performance Polymers Crastin® FG6130 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced High Viscosity Polybutylene Terephthalate Developed for Food Contact Applications and Extrusion and Injection Molding Crastin FG6130 NC010 is an unreinforced medium high viscosity polyb.. |
|||
Viscosity Test | 130 cm³/g | 130 cm³/g | ISO 307 1157 1628 |
DuPont Performance Polymers Crastin® S600F20 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S600F20 NC010 is an unreinforced lubricated medium viscosity polybutylene terephthalate resin for injection molding.Information provi.. |
|||
Viscosity Test | 130 cm³/g | 130 cm³/g | ISO 307 1157 1628 |
DuPont Performance Polymers Crastin® S600F20UV WT660 Polybutylene Terephthalate (PBT) Unreinforced UV Stabilized Polybutylene Terephthalate Crastin S600F20 NC010 is an unreinforced lubricated medium viscosity polybutylene terephthalate resin for injection molding.Information provided.. |
|||
Viscosity Test | 130 cm³/g | 130 cm³/g | ISO 307 1157 1628 |
DuPont Performance Polymers Crastin® S620F20 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S620F20 NC010 is an unreinforced nucleated lubricated medium viscosity polybutylene terephthalate resin for fast injection molding.In.. |
|||
Viscosity Test | 130 cm³/g | 130 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® 70G33HS1L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G33HS1L NC010 is a 33% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor.. |
|||
Viscosity Test | 130 cm³/g | 130 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® 70G43L NC010 Nylon 66
(Unverified Data**) 43% Glass Reinforced Polyamide 66Zytel 70G43L NC010 is a 43% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Viscosity Test | 130 cm³/g | 130 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® FE270038 BK267 Nylon 66
(Unverified Data**) 40% Glass/Mineral Reinforced Polyamide 66 Zytel FE270038 is a 40% glass fiber/mineral reinforced heat stabilized polyamid 66 for injection molding. It is well suited for water injection technology.I.. |
|||
Viscosity Test | 130 cm³/g | 130 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® RS LC1000 BK385 Nylon 1010 UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight... |
|||
Viscosity Test | 130 cm³/g | 130 cm³/g | Viscosity number |
BASF Ultramid® B3GM35 Q611 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid B3GM35 Q611 is a 40% combined glass-fiber and mineral reinforced injection molding PA6 grade. |
|||
Viscosity Test | 130 cm³/g | 130 cm³/g | Viscosity Number |
Arkema Group Lacovyl® PE 1311 H PVC LACOVYL PE 1311 H is a vinyl chloride homopolymer manufactured by emulsion polymerization process for the preparation of high viscosity plastisols. It is particularly suitable for the manufacture o.. |
|||
Viscosity Test | 130 cm³/g | 130 cm³/g | Viscosity number |
BASF Ultradur B 4500 PBT Ultradur B4500 is a general-purpose injection molding grade for high-precision, high-toughness, and dimensionally stable engineering parts. It conforms to FDA requirements of 21 CFR 177.1660. |
|||
Viscosity Test | 130 cm³/g | 130 cm³/g | Viscosity number |
BASF Ultradur B 4520 PBT Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade. |
|||
Viscosity Test | 130 cm³/g | 130 cm³/g | Viscosity number |
BASF Ultramid® B3GM35 Q611 15/25% Glass/Mineral Filled PA6 (Conditioned) Ultramid B3GM35 Q611 is a 40% combined glass-fiber and mineral reinforced injection molding PA6 grade. |