Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 80.0 - 145 cm³/g | 80.0 - 145 cm³/g | Average value: 110 cm³/g Grade Count:7 |
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% .. |
|||
Viscosity Test | 83.0 - 145 cm³/g | 83.0 - 145 cm³/g | Average value: 109 cm³/g Grade Count:3 |
Overview of materials for Nylon 612, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of .. |