Physical Properties | Metric | English | Comments |
---|---|---|---|
Carbon Dioxide Transmission | 80.0 cc-mm/m²-24hr-atm | 203 cc-mil/100 in²-24hr-atm | 23°C/0%r.h.; DIS 15105-1/-2 |
EMS-Grivory Grivory® F 34 NL PA6 Grilon F 34 NL nat. 6019 is a medium viscosity PA 6 containing nucleation and lubrication suitable for the production of coex blown films and mono or coex cast films. Grilon F 34 NL nat. 6019 has be.. |
|||
Carbon Dioxide Transmission | 80.0 cc-mm/m²-24hr-atm | 203 cc-mil/100 in²-24hr-atm | 23°C/0%r.h.; DIS 15105-1/-2 |
EMS-Grivory Grivory® F 47 H NL nat 6020 PA6 Product description: Grilon F 47 HNL natural 6020 is a nucleated, high viscosity polyamide 6. This product exhibits the following features: Good mechanical propertiesGood barrier against oils and fa.. |
|||
Carbon Dioxide Transmission | 80.0 cc-mm/m²-24hr-atm | 203 cc-mil/100 in²-24hr-atm | 23°C/0%r.h.; DIS 15105-1/-2 |
EMS-Grivory Grivory® FG 34 NL nat 6023 PA6 Product description: Grilon FG 34 NL natural 6023 is a modified, medium viscosity polyamide 6. Grilon FG 34 NL natural 6023 exhibits following improvements compared to a PA 6: Better gas barrier pro.. |
|||
Carbon Dioxide Transmission | 80.0 cc-mm/m²-24hr-atm | 203 cc-mil/100 in²-24hr-atm | 23°C/0%r.h.; DIS 15105-1/-2 |
EMS-Grivory Grivory® FG 40 NL nat 6018 PA6 Information provided by EMS Grivory |
|||
Carbon Dioxide Transmission | 80.0 cc-mm/m²-24hr-atm | 203 cc-mil/100 in²-24hr-atm | 23°C/0%r.h.; DIS 15105-1/-2 |
EMS-Grivory Grivory® FG 40 NL nat 6021 PA6 Product description: Grilon FG 40 NL natural 6021 is a modified, high viscosity polyamide 6. As a result of the modification in comparison to conventional polyamide 6 Grilon FG40 NL natural 6021 off.. |
|||
Carbon Dioxide Transmission | 80.0 cc-mm/m²-24hr-atm | 203 cc-mil/100 in²-24hr-atm | 23°C/0%r.h.; DIS 15105-1/-2 |
EMS-Grivory Grivory® FG 40 NL nat 6025 PA6 Product description: Grilon FG 40 NL natural 6025 is a modified, high viscosity polyamide 6. Compared to conventional polyamide 6 Grilon FG40 NL natural 6025 offers the following improvements:Better.. |
|||
Carbon Dioxide Transmission | 80.0 cc-mm/m²-24hr-atm | 203 cc-mil/100 in²-24hr-atm | 23°C/0%r.h.; DIS 15105-1/-2 |
EMS-Grivory Grivory® FG 47 NL nat 6028 PA6 Product description: Grilon FG 47 NL natural 6028 is a modified, high viscosity Polyamide 6, which contains also slip and nucleating agents. Grilon FG 47 NL natural 6028 shows following improvements.. |
|||
Carbon Dioxide Transmission | 80.0 cc-mm/m²-24hr-atm | 203 cc-mil/100 in²-24hr-atm | 23°C/0%r.h.; DIS 15105-1/-2 |
EMS-Grivory Grivory® F 40 NL PA6 Product description: Grilon F 40 NL natural 6018 is a nucleated and lubricated high viscosity polyamide 6. This product exhibits the following features: Good gas barrierGood mechanical propertiesGoo.. |
|||
Carbon Dioxide Transmission | 80.0 cc-mm/m²-24hr-atm | 203 cc-mil/100 in²-24hr-atm | 23°C/0%r.h.; DIS 15105-1/-2 |
EMS-Grivory Grivory® F 47 NL nat 6028 PA6 Product description: Grilon F 47 NL natural 6028 is a nucleated, high viscosity polyamide 6. This product exhibits the following features: Good gas barrierGood mechanical propertiesGood barrier agai.. |
|||
Carbon Dioxide Transmission | 80.0 cc-mm/m²-24hr-atm | 203 cc-mil/100 in²-24hr-atm | 23°C/0%r.h.; DIS 15105-1/-2 |
EMS-Grivory Grivory® BM 20 SBG PA* Product description: Grilon BM 20 SBG is a lactam free multipolyamide. Grilon BM 20 SBG has the following features: Lactam freeGood transparency and glossGood flexibility and toughnessVery good ther.. |
|||
Carbon Dioxide Transmission | 80.0 cc-mm/m²-24hr-atm | 203 cc-mil/100 in²-24hr-atm | 23°C/0%r.h.; DIS 15105-1/-2 |
EMS-Grivory Grivory® F 50 nat 6368 PA6 Product description: Grilon F 50 natural 6368 is a modified, very high viscous Polyamide 6 for extrusion processes: Very high melt strengthGood chemical resistanceGood gas-barrierGood mechanical pro.. |