Polymer Property : Density = 0.0348 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.957 - 0.963 g/cc

@Temperature 20.0 °C
0.0346 - 0.0348 lb/in³

@Temperature 68.0 °F
Kazanorgsintez PE2NT76-17 High Density Polyethylene for Blow Molding
Production Method: Gaseous-phase method. Application: Compositions are intended for goods produced by injection molding method.Information Provided by Kazanorgsintez
Density 0.956 - 0.962 g/cc

@Temperature 20.0 °C
0.0345 - 0.0348 lb/in³

@Temperature 68.0 °F
Kazanorgsintez PE2NT 11-9 High Density Polyethylene Composite
Production Method: Copolymerization of eythylene at low pressure in presence of complex catalysts using gaseous-phase method. Application: Composition is intended to be processed into pressure p..