Polymer Property : Density = 0.957 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.957 - 0.963 g/cc

@Temperature 20.0 °C
0.0346 - 0.0348 lb/in³

@Temperature 68.0 °F
Kazanorgsintez PE2NT76-17 High Density Polyethylene for Blow Molding
Production Method: Gaseous-phase method. Application: Compositions are intended for goods produced by injection molding method.Information Provided by Kazanorgsintez